Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 14.95 g/cc | 0.5401 lb/in³ | |
Goodfellow Tungsten Carbide/Cobalt Tungsten Carbide is a hard, brittle ceramic which, when combined with 6% to 10% Cobalt, forms a tough Cermet (Ceramic-Metal). This material was developed for use in cutting tools, having hard cerami.. |
|||
Density | 14.95 g/cc | 0.5401 lb/in³ | |
CoorsTek ACI-Ni6 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
Density | 14.95 g/cc | 0.5401 lb/in³ | |
China Tungsten YG6 Tungsten Carbide Information provided by China Tungsten |
|||
Density | 14.95 g/cc | 0.5401 lb/in³ | |
China Tungsten YG6A Tungsten Carbide Information provided by China Tungsten |
|||
Density | 14.95 g/cc | 0.5401 lb/in³ | |
China Tungsten YG6C Tungsten Carbide Information provided by China Tungsten |