Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 10.75 g/cc | 0.3884 lb/in³ | |
Indium Corp. Indalloy® 228 Pb-Sn-Ag Solder Alloy (Sn10) High temp solder. Not recommended for applications above 120°C, due to formation of eutectic.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 10.75 g/cc | 0.3884 lb/in³ | |
Indium Corp. Indalloy 242 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | 10.75 g/cc | 0.3884 lb/in³ | |
Indium Corp. Indalloy® 159 Pb-Sn Solder Alloy High temp solder for BGA applications.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 10.75 g/cc | 0.3884 lb/in³ | |
Williams Advanced Alloys WS290 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |