Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.58 g/cc | 0.310 lb/in³ | |
Performance Alloys MoldStar® 90 Copper Mold Alloy Description: MoldStar® 90 is a beryllium-free copper alloy for the blow molding and injection molding industries as well as other industrial applications. MoldStar® 90 provides a good balance of t.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | P/M (98%) |
Kennametal Stellite Stellite® STAR cast Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | P/M (98%) |
Kennametal Stellite Stellite® STAR with P/M Processing Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
Indium Corp. Indalloy 69 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
Indium Corp. Indalloy 75 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
H.C. Starck Grain Stabilized Niobium (GSNb) GSNb is a patent pending single-phase micro-alloy that has a grain size of approximately 2 ASTM numbers finer than standard commercial grade niobium.Applications: Grain Stabilized Niobium (GSNb) is.. |
|||
Density | 8.59 g/cc | 0.310 lb/in³ | |
Indium Corp. Indalloy 235 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.57 g/cc | 0.310 lb/in³ | |
Indium Corp. Indalloy® 282 57Bi/42Sn/1Ag Lead-Free Solder Alloy The addition of Ag adds mechanical strength. Good thermal fatigue performance; established history.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
LATI Latigray 82-03 CW/95 PA 12, Metallic Reinforced Radiopaque compound based on Polyamide 12 (PA12). Metallic filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Density | 8.59 g/cc | 0.310 lb/in³ | |
Goodfellow Niobium 99/Zirconium 1 Alloy High temperature alloy used in Sodium and Magnesium vapor lamp electrodes and for coating the inside of Stainless Steel 316 tubes to improve corrosion resistance. The alloy combines moderate strengt.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, 1/2 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, 1/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, 3/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, Annealed 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, Extra Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, Extra Spring 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, Spring 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C27450 Copper-Zinc Alloy Finished product available as wire or tube.Chicago Extruded Metal temper code: H04Information provided by Chicago Extruded Metals |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
ATI Wah Chang Nb/Nb Alloy Nb-I ZR Improved creep strength versus pure niobium. Replacement for pure niobium in applications requiring the chemical resistance of niobium and a material with high melting temperature.Information provid.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
AIM 58 Fusible Alloy Uses: lens blocking; proof casting; fusible element in safety devices; anchoring parts for machining; sealing adjustment screws; holding jet engine blades for machining and broaching; filler for sup.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
ATI Wah Chang Niobium Niobium is a soft, ductile metal which can be cold worked over 90 percent before annealing becomes necessary. In appearance, the metal is somewhat similar to stainless steel. The density of 8.57 gm/.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
Wall Colmonoy COLMONOY® 22 - Nickel Alloy With Tungsten Carbide Description and Application: A harder version of Colmonoy 23A and 24, for similar applications. Can be finished with a file.Method of Application: Oxyacetylene, FusewelderInformation provided by Wa.. |
|||
Density | 8.59 g/cc | 0.310 lb/in³ | |
Wall Colmonoy COLMONOY® 225 - Custom Formulated Nickel-Based Alloy For Glass Description and Application: Patented alloy specially designed for glass container mold protection and restoration. Also used for rebuilding automotive parts (clutch components).Method of Applicati.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
Wall Colmonoy COLMONOY® 226 - Custom Formulated Nickel-Based Alloy For Glass Patented alloy specially designed for glass container mold protection and restoration. Also used for rebuilding automotive parts (clutch components).Method of Application: FusewelderInformation pro.. |