Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.31 g/cc | 0.300 lb/in³ | |
Kennametal Stellite Stellite® 21 Excellent high temperature strength, high toughness. Solution treat at 1191-1204°C, rapid air cool, age between 538-871°C to increase hardness and strength at the expense of impact and ducti.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Materion BrushCAST® 20C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Materion BrushCAST® 21C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Special Metals INCONEL® G-3 Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Weartech International WT-40 Nickel Hardfacing & Wear Resistant Alloy Applications: glass industry plungers and mold componentsInformation provided by Weartech International |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Goodfellow Havar® High-Strength Non-Magnetic Cobalt-Base Alloy Co42.5/Cr20/Ni13/Fe/W/Mo/MnInformation provided by Goodfellow. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Strip, Heat Treated Heat Treatment 5 hours at 482°C. The strength and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, duc.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 10% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 47% Cold Reduction (Coil Spring Range), Heat Treated Heat Treatment 5 hours at 527°C. 45-48% cold reduction is the normal coil spring range. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below ar.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 65% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Bohler-Uddeholm BÖHLER S400(M7) High Speed Steel Description: High alloyed molybdenum high speed steel with good resistance and high toughness.Applications: Taps, twist drills, reamers, milling tools, broaches tools, cold extrusion dies.Standards:.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Ceradyne SEMICORE® S2-17B MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
ATI Allvac® Nickelvac® X-750 Nickel Superalloy, Heat Treatment: 1149°C (2100°F) + Age Data provided by Allvac.Applications: Turbine, engine components. Blades, vanes, fasteners, springs, bellows. Extrusion dies, nuclear, heat treating, forming tools. |
|||
Density | 8.31 g/cc | 0.300 lb/in³ | |
Kennametal Stellite Stellite® 25 Cobalt Chromium Cast Alloy Stellite alloy 25 forms a protective oxide film during hot metal-on metal wear which prevents metal transfer and damage due to adhesion. The alloy is resistant to thermal cracking and surface fatig.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Ceradyne SEMICORE® S2-17A MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Elgiloy® Co-Cr-Ni Alloy, Wire The strength and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fatigue life, and.. |
|||
Density | 8.30 g/cc | 0.300 lb/in³ | |
Resistalloy International Resistalloy 8020 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |