Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.264 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 7.30 g/cc
0.264 lb/in³
Indium Corp. 6N5 High Purity Indium Metal
High purity Indium is used as the starting material in the manufacture of indium based group III-V such asIn/PIn/AsIn/SbIn/Ga/AsIn/Ga/As/P These compound semiconductors find use in ultra high effici..
Density 7.32 g/cc
0.264 lb/in³
Indium Corp. Indalloy 160 Tin Solder Alloy
Information Provided by Indium Corporation
Density 7.30 g/cc
0.264 lb/in³
Indium Corp. Indalloy 71 Indium-Tin Solder Alloy
Information Provided by Indium Corporation
Density 7.30 g/cc
0.264 lb/in³
Indium Corp. Indalloy 87 Indium-Tin Solder Alloy
Information Provided by Indium Corporation
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy 90 Indium Solder Alloy
Information Provided by Indium Corporation
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy® 244 99.3Sn/0.7Cu Lead-Free Solder Alloy
Inexpensive. Alloy of choice for general wave solder assembly.Information provided by the manufacturer, Indium Corporation.
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy® 4 Pure Indium Solder
Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogeni..
Density 7.32 g/cc
0.264 lb/in³
Indium Corp. Indalloy 258 Tin Solder Alloy
Information Provided by Indium Corporation
Density 7.30 g/cc
0.264 lb/in³
Indium Corp. Indalloy® 1E In-Sn Solder Alloy
Lowest melting point practical solder. Indium-tin eutectic with sharp melting point. Has good wettability on glass, quartz and many ceramics. Has good low temperature malleability and therefore com..
Density 7.32 g/cc
0.264 lb/in³
Indium Corp. Indalloy® 262 Tin-Copper Solder Alloy
Information provided by the manufacturer, Indium Corporation of America.
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy® 263 Tin-Silver-Copper Solder Alloy
Information provided by the manufacturer, Indium Corporation of America.
Density 7.30 g/cc
0.264 lb/in³
Coating Property
The NanoSteel® Company SHS 8000 TWAS Iron Based Alloy, Cored Wire
Coating Description: SHS 8000 TWAS is a glass forming iron based alloy that forms a nanocomposite comprised of a mixed amorphous and nanoscale microstructure when sprayed as a coating. SHS 8000 fea..
Density 7.30 g/cc
0.264 lb/in³
United Cast Bar Unibar 300 Continuously Cast Iron
Unibar 300 is alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and an excellent surface finish..
Density 7.30 g/cc
0.264 lb/in³
United Cast Bar Unibar 350 Continuously Cast Iron
Unibar 350 is a special grade alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and producing a..
Density 7.30 g/cc
0.264 lb/in³
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Density 7.30 g/cc
0.264 lb/in³
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron
Offers higher wear resistance, strength & heat-treatment response while still possessing good machinability and excellent surface finishes. Noise and vibration damping are good in this grade.Unibar ..
Density 7.30 g/cc
0.264 lb/in³
United Cast Bar Unibar 600-3 Continuously Cast Spheroidal Graphite Iron
Offers reasonable machinability and excellent surface finish combined with higher wear resistance, strength & heat treatment. Noise and vibration damping are good in this grade.Unibar 600-3 can be ..
Density 7.30 g/cc
0.264 lb/in³
United Cast Bar Unibar 700-2 Continuously Cast Spheroidal Graphite Iron
Offers higher wear resistance; strength & heat-treatment response while still possessing reasonable machinability and excellent surface finish. Noise and vibration damping are good in this grade.Uni..
Density 7.30 g/cc
0.264 lb/in³
Williams Advanced Alloys WS118 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 7.30 g/cc
0.264 lb/in³
Williams Advanced Alloys WS145 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 7.31 g/cc
0.264 lb/in³
American Elements Indium Nanoparticles
General DescriptionIndium (In) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Indium Particles are typically 20-40 nanomete..
Density 7.31 g/cc
0.264 lb/in³
California Fine Wire Stablohm 750 Chromium, Aluminum, and Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Density 7.30 g/cc
0.264 lb/in³
Alliance A-3 Alnico Magnetic Material
Density 7.30 g/cc
0.264 lb/in³
AIM 52In/48Sn Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Density 7.30 g/cc
0.264 lb/in³
Alliance A-5 Alnico Magnetic Material
Density 7.30 g/cc
0.264 lb/in³
Alliance A-5DG Alnico Magnetic Material
Density 7.30 g/cc
0.264 lb/in³
Alliance A-6 Alnico Magnetic Material
Density 7.30 g/cc
0.264 lb/in³
Alliance A-8 Alnico Magnetic Material
Density 7.30 g/cc
0.264 lb/in³
Indium Corp. 3N Commercial Indium Metal
Indium is a versatile metal with unique physical properties.Indium has one of the widest liquid temperature ranges of any metal.Indium has a low vapor pressure, making it ideal for high vacuum appli..
Copyright © lookpolymers.com All Rights Reserved