Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials F-240-S Steel Powdered Metal Applications:Medium stressed mechanical componentsEquivalent MPIF Specification: F-0005-25All information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials F-240-S(HT) Steel Powdered Metal Applications:Medium stressed mechanical componentsEquivalent MPIF Specification: F-0005-60(HT)All information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials F-241-S Iron Powdered Metal Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-15All information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials F-244-S(HT) High Carbon Steel Powdered Metal Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-85(HT)All information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials FCC-214-S High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials FCC-214-S(HT) High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials FN-253-S(HT) 4600 Powdered Metal High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-100HTAll information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials FN-255-S Nickel Steel Powdered Metal Good impact resistant mechanical components. Good hardenability.Equivalent MPIF Specification: FN-0205-25All information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials FN-255-S(HT) Nickel Steel Powdered Metal Good impact resistant mechanical components. Good hardenability.Equivalent MPIF Specification: FN-0208-130HTAll information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
Pacific Sintered Materials FN-262-S High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-35All information provided by Pacific Sintered Metals. |
|||
Density | >= 6.80 g/cc | >= 0.246 lb/in³ | |
Pacific Sintered Materials SS-316-SH 316L Stainless Steel Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.All information provided by Pacific Sintered Metals. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals 4600 FN-253-S(HT) Powdered Metal High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FL-4605-100HTInformation Provided by Pacific Sintered Metals, a division of PSM .. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-214-S Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals High Carbon Steel F-244-S(HT) Powdered Metal Highly stressed mechanical components, Good hardenability Equivalent MPIF Specification: F-0008-85(HT)Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.80 - 7.00 g/cc | 0.246 - 0.253 lb/in³ | |
PSM Industries Pacific Sintered Metals Iron F-241-S1 Powdered Metal DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type III, Class AInformation Provided by Pacific Sintered Metals, a .. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Nickel Steel FN-255-S Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0205-25Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Steel F-240-S(HT) Powdered Metal Medium stressed mechanical components Equivalent MPIF Specification: F-0005-60(HT)Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.80 g/cc | 0.246 lb/in³ | |
PSM Industries Ferro-TiC® SK Impact Resistant Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Exce.. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Iron F-241-S Powdered Metal Low stressed mechanical components, Soft magnetic applications Equivalent MPIF Specification: F-0000-15Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Nickel Iron FN-250-S Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0200-20Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Nickel Steel FN-255-S(HT) Powdered Metal Good impact resistant mechanical components, Good hardenability Equivalent MPIF Specification: FN-0208-130HTInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 6.80 g/cc | 0.246 lb/in³ | |
MMCC Copper/Graphite Fiber GC 7-340 Metal Matrix Composite Discontinuous graphite fiber copper product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plated,.. |
|||
Density | 6.80 g/cc | 0.246 lb/in³ | |
American Elements Neodymium Nanoparticles General DescriptionNeodymium (Nd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Neodymium Particles are typically 10 - 45 nanometers (nm) with spec.. |
|||
Density | >= 6.80 g/cc | >= 0.246 lb/in³ | |
China Tungsten STG10-15 PM Structural Parts Information provided by China Tungsten |
|||
Density | >= 6.80 g/cc | >= 0.246 lb/in³ | |
China Tungsten STG60-25 PM Structural Parts Information provided by China Tungsten |
|||
Density | >= 6.80 g/cc | >= 0.246 lb/in³ | |
China Tungsten STG60Cu3Mo55 PM Structural Parts Information provided by China Tungsten |
|||
Density | 6.80 - 7.40 g/cc | 0.246 - 0.267 lb/in³ | |
China Tungsten ST2270 PM Antifriction Parts Information provided by China Tungsten |
|||
Density | >= 6.80 g/cc | >= 0.246 lb/in³ | |
China Tungsten STG90-30 PM Structural Parts Information provided by China Tungsten |
|||
Density | 6.80 g/cc | 0.246 lb/in³ | |
Ametek P304L P/M Stainless Steel, Sintered from 6.7 g/cc Green Density Powder apparent bulk density 2.7 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for .. |
|||
Density | 6.80 - 7.20 g/cc | 0.246 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-S Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-35Information Provided by Pacific Sintered Metals, a division.. |