Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.68 - 3.72 g/cc | 0.133 - 0.134 lb/in³ | Sintered |
Nabaltec GRANALOX® NM 9212 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |
|||
Density | 3.68 - 3.72 g/cc | 0.133 - 0.134 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9212 E Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.67 g/cc | 0.133 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 313 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.68 g/cc | 0.133 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton 504 Mullite Brand 504 features: Max spall resistance.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when t.. |
|||
Density | 3.67 g/cc | 0.133 lb/in³ | |
MarkeTech Sodium Iodide:Thallium (Nal:Tl) Scintillator Crystal Sodium iodide activated by thallium has long been the scintillation standard. Nal:Tl has good performance, economical price, high luminescence efficiency, very good spectroscopic performance and no .. |
|||
Density | 3.67 g/cc | 0.133 lb/in³ | |
GBC Grade 96 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Density | 3.68 g/cc | 0.133 lb/in³ | |
Ferro CF 7574 Glaze and Sealant Glass Glass Type: Zn-B-Si Typical Powder Form: VSD Typical Application: Pyrex Silicon Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and .. |
|||
Density | 3.68 g/cc | 0.133 lb/in³ | |
Schott N-FK51A Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Density | 3.69 g/cc | 0.133 lb/in³ | |
Schott N-LAK10 Glass Information Provided by SCHOTT North America, Inc. |