Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.35 g/cc | 0.121 lb/in³ | Apparent |
Gouda Vuurvast AC 85-10 D Dense Refractory Brick Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te.. |
|||
Density | 3.35 g/cc | 0.121 lb/in³ | Apparent |
Gouda Vuurvast AC 90-8 Dense Refractory Brick Description: Excellent resistance against alkali- and metal slags. The 8% chromium-oxide addition gives good volume stability at very high temperatures. Applications: chemical incinerators, combusti.. |
|||
Density | 3.35 g/cc | 0.121 lb/in³ | ASTM D792 |
Techmer ES Plastiblend® PPS 05003 Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite Features: LubricatedUnoriented Magnetic:Residual Induction, BR: 1100 GaussCoercive Force, Hc: 750 OerstedsIntrinsi.. |
|||
Density | 3.35 g/cc | 0.121 lb/in³ | |
CeramTec ALUTIT® S Aluminum Titanate (Strength Optimized) ALUTIT®, which is produced in a special reaction-sintering process, consists of high-purity aluminum oxide and titanium oxide. It offers excellent resistance to sudden changes in temperature, good .. |
|||
Density | 3.36 g/cc | 0.121 lb/in³ | |
Ceradyne Ceralloy® 7712 Al2O3-SiC Applications:slot mode absorbersInformation provided by Ceradyne Company |
|||
Density | 3.35 g/cc | 0.121 lb/in³ | Apparent |
Gouda Vuurvast LP 100 Dense Refractory Brick Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qual.. |
|||
Density | 3.35 g/cc | 0.121 lb/in³ | Apparent |
Gouda Vuurvast LP 97-3 Dense Refractory Brick Description: A high alumina quality brick containing a limited percentage of chromium oxide for improved slag resistance. The product has a very low silica- and iron oxide percentage so that it can .. |