Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.88 g/cc | 0.104 lb/in³ | |
Pyrotek Pyrocast PT-190 Refractory Cast Parts Pyrocast PT-190 is an extremely dense alumina based refractory. It is best suited for applications where high velocity metal erosion potential is a problem, due to its strength and abrasion resista.. |
|||
Density | 2.88 g/cc | 0.104 lb/in³ | |
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part.. |
|||
Density | 2.88 g/cc | 0.104 lb/in³ | |
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part.. |
|||
Density | 2.89 g/cc | 0.104 lb/in³ | |
Schott VG14 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Density | 2.87 g/cc | 0.104 lb/in³ | |
Schott VG9 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Density | 2.89 g/cc | 0.104 lb/in³ | |
Schott N-BAF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.88 g/cc | 0.104 lb/in³ | |
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us.. |
|||
Density | 2.87 - 2.97 g/cc | 0.104 - 0.107 lb/in³ | Fired |
CeramTec Ceramtape GC Glass Ceramic LTCC (Low Temperature Cofired Ceramic) is a new type of ceramic film developed by CeramTec AG's Electronics division. With the aid of these ceramics and their almost shrinkage-free sintering process.. |