Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.51 g/cc | 0.0907 lb/in³ | |
Mateck Glass (BK7 Schott or analogous) Optical crystals |
|||
Density | 2.51 g/cc | 0.0907 lb/in³ | |
Schott WG280 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |
|||
Density | 2.51 g/cc | 0.0907 lb/in³ | |
Schott D 263 Thin Borosilicate Glass D 263 is a low alkali borosilicate glass that is produced by melting the purest raw materials. As such, it is very resistant to chemical attack. D 263, with its specific properties and large rang.. |
|||
Density | 2.51 g/cc | 0.0907 lb/in³ | |
Schott D 263® T eco Thin Borosilicate Optical Glass D 263® T eco thin glass is a clear borosilicate glass that has a high chemical resistance and is produced by the down-draw method. It is available in a variety of thicknesses ranging from 0.03 mm.. |
|||
Density | 2.51 g/cc @Temperature 25.0 °C |
0.0907 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8405 UV-transmitting Glass Sodium-potassium-barium-silicate glass, highly UV-transmitting Used as envelope for germicidal lamps (low-pressure mercury vapor discharge lamps) and for UV detectors The heavy metal content for t.. |
|||
Density | 2.51 g/cc | 0.0907 lb/in³ | |
Schott N-BK7 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.51 g/cc | 0.0907 lb/in³ | |
Schott Nextrema® 712-6 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Density | 2.51 g/cc | 0.0907 lb/in³ | |
Schott Nextrema® 724-5 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Density | 2.51 g/cc | 0.0907 lb/in³ | |
Schott WG295 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |