Polymer Property : Density = 0.0835 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.31 g/cc
0.0835 lb/in³
calculated from bulk density after subtracting pore volume
MarkeTech Repton 902 Cordierite Mg-Al-Si Oxide
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa..
Density 2.31 g/cc

@Temperature 25.0 °C
0.0835 lb/in³

@Temperature 77.0 °F
Schott Glass 8245 Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and molybdenum, minimum X-ray absorption, low self radiation, good insulator X-ray tubes, video-frequency tubes, photomultiplier tubes The heavy metal..
Density 2.31 g/cc
0.0835 lb/in³
ASTM D792
Techmer ES HiFill® PPS 0231 B LE
Availability: North AmericaForms: PelletsFeatures: High Density and Low ExtractablesAppearance: OpaqueInformation provided by TP Composites, Inc.
Density 2.31 g/cc
0.0835 lb/in³
ASTM D792 Method A
Arlon CuClad 250 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 250 uses a higher fiberglass/PTFE ratio to provide mechanical properties approaching those of conventional substrates. Better dimensional stability and lower thermal expansion in all directi..
Density 2.31 g/cc
0.0835 lb/in³
ASTM D792 Method A
Arlon DiClad 522/527 PTFE/Woven Fiberglass Laminates
DiClad 522 and DiClad 527 use a higher fiberglass/PTFE ratio to provide mechanical properties approaching conventional substrates.Extremely Low Loss TangentExcellent Dimensional StabilityProduct Per..