Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.25 g/cc | 0.0813 lb/in³ | Green Density |
Nabaltec NABALOX® NO 115 TC Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | Green Density |
Nabaltec NABALOX® NO 115-71 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPC B10075 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPC B8075 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH B8075 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | Apparent |
Gouda Vuurvast AK 42 Dense Refractory Brick Description: Because of its abrasion resistance and high density, this brick performs very well in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were c.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | Apparent |
Gouda Vuurvast B 1 Sp Dense Refractory Brick Description: High mechanical strength and very low porosity are typical for this type of brick. Application: transition zone in cement kilns, incinerators, steel ladles.Remarks: This data represents.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | Theoretical |
Momentive Performance Materials PolarTherm® PT110 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | Theoretical |
Momentive Performance Materials PolarTherm® PT120 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | Apparent |
Gouda Vuurvast A 1 S Dense Refractory Brick Description: A brick with a high creep resistance, successfully applied in anode baking furnaces and in the transition zone of rotary cement kilns.Remarks: This data represents average values, obtai.. |
|||
Density | 2.25 g/cc @Temperature 25.0 °C |
0.0813 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8448 Intermediate Sealing Glass Intermediate sealing glass Sealing to the glasses 8330, 8449, 8486, 8487, and tungstenInformation provided by SCHOTT AG. |
|||
Density | 2.25 g/cc @Temperature 25.0 °C |
0.0813 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8687 Borosilicate Glass Borosilicate glass for sealing to tungsten, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | |
SGL Carbon Group EK 3205 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ASTM D792 |
Techmer ES HiFill® PP 0225 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® 488 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® 641 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® LR Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ± 0.01, True Density |
Sinotek Materials ZSG-15 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ± 0.01, True Density |
Sinotek Materials ZSG-23 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ± 0.01, True Density |
Sinotek Materials ZSG-12 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ± 0.01, True Density |
Sinotek Materials ZSG-17 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ± 0.01, True Density |
Sinotek Materials ZSG-20 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Density | 2.25 - 2.35 g/cc | 0.0813 - 0.0849 lb/in³ | |
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | Theoretical |
Momentive Performance Materials PolarTherm® PT140 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | Theoretical |
Momentive Performance Materials PolarTherm® PT160 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | Theoretical |
Momentive Performance Materials PolarTherm® PT180 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | Theoretical |
Momentive Performance Materials PolarTherm® PT370 Boron Nitride (BN) Powder Low Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic compon.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | Theoretical |
Momentive Performance Materials PolarTherm® PT620 Boron Nitride (BN) Powder High Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Density | 2.25 g/cc | 0.0813 lb/in³ | ± 0.01, True Density |
Sinotek Materials ZSG-25 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |