Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.22 g/cc | 0.0802 lb/in³ | |
Solvay Specialty Polymers Polymist® XPH-284 PTFE Powder Lubricant
(discontinued **) Meets the requirements of 21 CFR 177.1550.Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-u.. |
|||
Density | 2.22 g/cc | 0.0802 lb/in³ | ASTM D792 |
3M Dyneon™ CC604 PTFE, 20% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Density | 2.22 g/cc | 0.0802 lb/in³ | ASTM D4894 |
3M Dyneon™ CC605 PTFE 25% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Density | 2.22 - 2.24 g/cc | 0.0802 - 0.0809 lb/in³ | extruded; ASTM D792 |
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |
|||
Density | 2.22 g/cc | 0.0802 lb/in³ | Real Density |
SGL Carbon Group CF 3100 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 2.22 g/cc @Temperature 25.0 °C |
0.0802 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8337B Borosilicate Glass Borosilicate glass for sealing to Kovar metal and tungsten, highly UV-transmitting photomultiplier and UV detectors The heavy metal content for the elements lead, cadmium, mercury, and hexavalent .. |
|||
Density | 2.22 g/cc | 0.0802 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP) LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s). |
|||
Density | 2.22 g/cc | 0.0802 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® AR Bearing/Seal PTFE Rulon® AR is somewhat more flexible than Rulon® LR, hence suitable for seals and bonded coating of slide surfaces. It has many decades of use in automotive shaft seals and fuel metering pump c.. |
|||
Density | 2.22 g/cc | 0.0802 lb/in³ | Cured |
Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied b.. |
|||
Density | 2.22 g/cc | 0.0802 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Algoflon® 15GL PTFE; Glass Fiber Filled
(discontinued **) Data provided by the manufacturer.15 wt.% Glass Fiber. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almos.. |