Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.07 g/cc | 0.0748 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 4246 PTFE 35% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Density | 2.07 g/cc | 0.0748 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP ZX08005 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZX08005 is a Compound based on PPE + PS Blend resin, containing Mineral. Added features include: Improved Dielectric Properties. |
|||
Density | 2.07 g/cc | 0.0748 lb/in³ | ASTM D792 |
Plenco 1508 Polyester, Briquette, Injection Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Density | 2.07 g/cc | 0.0748 lb/in³ | ASTM D792 Method A |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |
|||
Density | 2.07 - 2.27 g/cc | 0.0748 - 0.0820 lb/in³ | Molded |
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig.. |