Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.593 g/cc | 0.05755 lb/in³ | |
Arlon CP-338R Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |