Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.474 - 1.479 g/cc | 0.05325 - 0.05343 lb/in³ | |
Solvay Chemicals E9000 Chloroform Chloroform is a non-flammable product.EINECS Number: 200-663-8/CAS Number: 67-66-3/UN number: 1888Information provided by Solvay |
|||
Density | 1.474 g/cc @Temperature 110 °C |
0.05325 lb/in³ @Temperature 230 °F |
|
Solvay Chemicals Perchloroethylene Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay |
|||
Density | 1.474 g/cc | 0.05325 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT LNP THERMOTUF* WF006I is a compound based on PBT containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
Density | 1.474 g/cc | 0.05325 lb/in³ | |
Arlon CP-368 Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Density | 1.474 g/cc | 0.05325 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg.. |