Polymer Property : Density = 0.04736 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.311 g/cc
0.04736 lb/in³
CRP Technology Windform® LX 2.0 Polyamide Composite
Processed by selective laser sintering (SLS). Windform® LX 2.0 has improved the already excellent performances of Windform® LX and this can be noticed from technical properties and sinterability ..