Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.15 g/cc | 0.0416 lb/in³ | |
Sika Industry SikaTack UltraFast Fast Cure One Part Polyurethane Adhesive Sika UltraFast SikaTack Fast Cure One Part Polyurethane AdhesiveThis revolutionary product uses heat instead of moisture to "pre-cure" the adhesive. The product is heated before applications using a.. |
|||
Density | 1.15 - 1.16 g/cc | 0.0416 - 0.0419 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6XAU High Heat Cast Nylon 6 (PA6) VEKTON® 6XAU is a high heat weather resistant cast nylon 6 with superior fatigue-resistant and bearing properties.General Vekton® Cast Nylon Information: VEKTON cast nylon, available in a variety .. |
|||
Density | 1.15 - 1.16 g/cc | 0.0416 - 0.0419 lb/in³ | ASTM D792 |
Ensinger Tecast™ 6PA Natural Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Natural is an FDA-compliant grade used in applications requiring cast nylon but without any fillers.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of.. |
|||
Density | 1.15 - 1.16 g/cc | 0.0416 - 0.0419 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6) Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combina.. |
|||
Density | 1.15 - 1.16 g/cc | 0.0416 - 0.0419 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6PA Blue Unfilled Cast Nylon 6 (PA6) Tecast 6PA Blue is a blue cast nylon with properties similar to natural nylon 6.General Tecast Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of go.. |
|||
Density | 1.15 - 1.17 g/cc | 0.0416 - 0.0423 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6PAL Oil-Filled Cast Nylon 6 (PA6) Tecast® 6PAL is used in applications requiring excellent bearing and wear properties where external lubrication is difficult or impractical.General Tecast® Cast Nylon Information: Tecast cast nylo.. |
|||
Density | 1.15 g/cc | 0.0416 lb/in³ | P |
Aremco Ceramacast™ 905 Silicon-Ceramic Potting Compound Ceramacast™ 905 is a silicone-bonded, ceramic filled high temperature adhesive and potting compound. |