Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.988 g/cc | 0.0357 lb/in³ | ASTM D792 |
Mytex Polymers AS78L(W)-GM-02 Polypropylene, Rubber modified, Compounded Description: AS78L(W)-GM-02 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties.Key Applications: Bumper fascias and all other exterior partsInform.. |
|||
Density | 0.989 g/cc @Temperature 20.0 °C |
0.0357 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell Glycol Ether DE Diethylene glycol ethyl ether Information provided by Lyondell. |
|||
Density | 0.989 - 1.04 g/cc | 0.0357 - 0.0376 lb/in³ | 309-2D Hardener |
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh.. |
|||
Density | 0.989 g/cc | 0.0357 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA350 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low viscosity adhesive, high strength, especially suitable for battery case applications.Informati.. |
|||
Density | 0.988 g/cc | 0.0357 lb/in³ | |
BASF 2-Ethylhexyl Choroformate Formula: C9H17ClO2CAS: 24468-16-1Description: 2-Ethylhexyl Chloroformate is a colorless to yellowish liquid with a pungent odor. It hydrolyzes in the presence of water.Synonyms: Chloroformic acid 2.. |
|||
Density | 0.987 g/cc | 0.0357 lb/in³ | ASTM D792 |
Multibase Multi-Flam™ 1502 PP Black Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |