Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM500LN Polypropylene, Impact Copolymer, High Flow, Medium Impact, Nucleated, Lube, Injection Molding COPYLENE™ CM500LN is a very high melt flow, medium impact polypropylene copolymer resin, designed for injection molding applications requiring a good balance of properties with faster cycling capab.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR020CL Polypropylene Impact Copolymer COPYLENE® CR020CL is a random copolymer formulated with advanced clarifier technology and with antistat and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH020 Polypropylene, Homopolymer, BOPP COPYLENE™ CH020 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches; Raffia/Tapes/Strapping; Peelable.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH020-02 Polypropylene, Thermoforming, Sheet, Film COPYLENE™ CH020-02 is a polypropylene homopolymer resin suitable for thermoforming, sheet and film fiber applications. Applications: Opaque Containers. Equivalent to Pro-fax® HL783HInformation pro.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH020-03 Polypropylene, Homopolymer, BOPP COPYLENE™ CH020-03 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applicationsApplications: Bags & Pouches, Raffia/Tapes/Strapping, Peelabl.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH023NX Polypropylene, Homopolymer, Thermoforming COPYLENE™ CH023NX has a high performance nucleation system designed to yield high clarity thermoformed articlesApplications: ThermoformingInformation provided by Phillips 66. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH043EW Polypropylene, Homopolymer, Slit Film, LWCO, Cordage COPYLENE™ CH043EW is a medium flow polypropylene homopolymer resin suitable for general injection molding or extrusion applications. Applications: Raffia/tapes/strapping. Equivalent to Pro-fax® HL.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH050 Polypropylene, Homopolymer, Cast Film BOPP COPYLENE™ CH050 is a polypropylene controlled rheology homopolymer resin designed for Cast Film BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches, Pe.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH085S Polypropylene, Homopolymer, Cast Film, Slip COPYLENE™ CH085S is a controlled rheology polypropylene homopolymer resin containing slip additive. COPYLENE™ CH085S is used in injection molding and cast film extrusion applications. Applications.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH350 Polypropylene Homopolymer COPYLENE™ CH350 is a controlled rheology, barefoot homopolymer designed for application as a base resin for compounding, consumer products and other injection molding applications.Applications: Inj.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM015 Polypropylene Impact Copolymer COPYLENE™ CM015 is low melt flow impact copolymer with a barefoot additive package and is designed for excellent processing in injection molding and extrusion applications.Applications: Injection M.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
LyondellBasell Moplen EP/60 Bianco Polypropylene Copolymer Description: Moplen Coat EP/60 Bianco fractional melt flow, 1,200 MPa flexural modulus, extrusion grade polypropylene copolymer has a very good balance of properties and processability. Available in.. |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
M. Holland Company CP710 Polypropylene Impact Copolymer AntistaticImpact copolymerGood flowGood impact resistanceNucleatedApplications: ClosuresHousehold goodsThin-walled parts |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Flint Hills P9H8M-058X Specialty Polypropylene Features: Does not contain animal derived components. Product is Phthalate-free. A low phosphorus content material.Applications: Extrusion coating. Suitable for silicone coating.Information pro.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | |
Mitsui EXCEREXâ„¢ 48070B(T) Polymer Processing Aid EXCEREXâ„¢ is an innovative processing improvement agent created with metallocene catalysis technology. EXCEREXâ„¢ gains in a number of ares simultaneously, including faster processing speeds.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ISO 1183 |
ExxonMobil EXACT™ 0210 Ethylene-based Plastomer for Multilayer Film Applications Exact 0210 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for seal layers in multilayer film applications requiring good flow/caul.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ISO 1183 |
ExxonMobil EXACT™ 0230 Plastomer for Multilayer Film Applications Product Description: Exact 0230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for both monolayer and multilayer co-extruded cast .. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | |
Dow AFFINITY™ PL 1880 Polyolefin Plastomer AFFINITY® PL 1880 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding packaging applications including high-speed, form-fill seal products. AFFINITY PL.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | |
Dow AFFINITY™ SM 1300 Polyolefin Plastomer AFFINITY® SM 1300 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in high clarity durable injection molded industrial and consumer goods and compression molded closu.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM-D792 |
Braskem PRA 0852 RACO Random Polypropylene Copolymer PRA 0852 is a medium melt flow rate random copolymer with slip and antiblocking agents. It is suitable for blown and cast film extrusion. PRA 0852 has excellent optical properties and good processab.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Bapolene® PP5052 Polypropylene, Injection Grade Polypropylene injection impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA standards for food.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | |
Arkema Group Appryl® 7280 Polypropylene - Polyethylene Copolymer PP/PE copolymer colored directly or during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive i.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792A |
Braskem RP 144 Coating Polypropylene Description: RP 144 is a high melt flow rate random copolymer, designed for high speed coating equipments. This product features good processability, excellent gloss and weldability.Applications: Wa.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Huntsman Rexell® V8401 Cast Film Extrusion LLDPE
(discontinued **) Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent combination of flexibility, flex crack resistance, and low temperature properties. It also exhibits excell.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH014 Polypropylene, Homopolymer, Extrusion, Strapping COPYLENE™ CH014 is a polypropylene homopolymer resin designed for extrusion applications. Applications: Raffia/Tapes/Strapping; Geotextile & Agriculture; Nets. Equivalent to Pro-fax® HL781GInforma.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CR300CL-01 Polypropylene Random Copolymer COPYLENE® CR300CL-01 is a reactor grade, clarified random copolymer specially designed and formulated for clear injection molding applications and is formulated with anti-stat for excellent mold re.. |
|||
Density | 0.903 g/cc @Temperature 15.0 °C |
0.0326 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil HD Plus 85W-140 Mobilube HD Plus 80W-90 and 85W-140 are extra high performance commercial gear lubricants formulated from select base oils and an advanced additive system. These lubricants are engineered for perfor.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | |
BASF N-Methylpiperazine Formula: C5H12N2CAS: 109-01-3Description: N-Methylpiperazine is a colorless to yellow liquid with an amine-like odor. It is miscible in water. Synonyms: 1-Methylpiperazine, N-MethylpiperazinApplica.. |
|||
Density | 0.902 g/cc | 0.0326 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CM090L Polypropylene, High Impact Copolymer CM090L is a high impact copolymer with antistat and is specially designed to excel in injection molding processes for consumer products.Applications: Injection MoldingInformation provided by Phillip.. |
|||
Density | 0.901 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Amco PRIMATOP PP CO 220-23 Impact Polypropylene Copolymer PP CO 220-23 has easy mold flow and excellent dimensional stability. Applications include closures, housewares, and small appliance applications.Former A-Top Polymers product; part of Amco product l.. |