Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.896 g/cc | 0.0324 lb/in³ | ASTM D792 |
Network Polymers NPP 25-0216 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.897 g/cc | 0.0324 lb/in³ | |
Pyrotek Pyroboard™ S1100 Roller Pyroboard™ S1100 is an economical material that is perfect for one time use on new campaigns.Information provided by Pyrotek. |
|||
Density | 0.897 g/cc | 0.0324 lb/in³ | ASTM D792 |
SABIC PP 651H Polypropylene Random Copolymer for PIPE Product Description: PP 651H is specially designed for transport of hot and cold drinking water. This grade is highly heat stabilized and specially formulated for extraction resistance.Typical App.. |
|||
Density | 0.898 - 0.904 g/cc | 0.0324 - 0.0327 lb/in³ | |
Kazanorgsintez Butyl Cellosolve, Industrial, Ethyleneglycolmonobutylether Production Method: OxyethylationInformation Provided by Kazanorgsintez |
|||
Density | 0.898 g/cc | 0.0324 lb/in³ | ASTM D1505 |
Ineos R01A-00 Polypropylene Random Copolymer Random copolymer R01A-00 is an antistatic polypropylene produced by a unique catalyst technology. It is designed for blow molding and extrusion applications and exhibits good stiffness and improved .. |
|||
Density | 0.898 g/cc | 0.0324 lb/in³ | ASTM D1505 |
Ineos R01A-01 Polypropylene Copolymer, Antistatic An antistated polypropylene random copolymer produced by Ineos utilizing unique catalyst technology. It is designed for blowmolding and extrusion applications and exhibits good stiffness and improv.. |
|||
Density | 0.898 g/cc | 0.0324 lb/in³ | ASTM D1505 |
Ineos R05C-00 Polypropylene Random Copolymer Random copolymer R05C-00 is an antistatic, clarified polypropylene random copolymer produced by a unique catalyst technology. It is designed as a high gloss resin and exhibits good stiffness and imp.. |
|||
Density | 0.897 g/cc | 0.0324 lb/in³ | ASTM D1505 |
LyondellBasell DP 8220M Polybutene Key Features: semi-crystalline, medium ethylene content random copolymer, reduces seal initiation temperature, FDA acceptableApplications: seal-peel layer of BOPP filmMeets FDA requirements in 21 CF.. |
|||
Density | 0.897 g/cc | 0.0324 lb/in³ | ASTM D792 |
Styron INSPIREâ„¢ T710-25 ES PolyPropylene Resin DA Thermoplastic Polyolefin Dow T710-25 ES Polypropylene Resin DAâ„¢ is a high impact TPO with enhanced flow, scratch and mar, and surface aesthetics for excellent molded-in-color appearance for automotive interior applicat.. |
|||
Density | 0.896 g/cc @Temperature 15.0 °C |
0.0324 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 50 1650 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |
|||
Density | 0.897 g/cc @Temperature 15.6 °C |
0.0324 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 120 Exxon Aviation Oil Aviation Oil 100, 120 and 20W-50 are non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxid.. |
|||
Density | 0.898 g/cc @Temperature 15.0 °C |
0.0324 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 50 Exxon XD-3 Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d.. |
|||
Density | 0.897 g/cc @Temperature 15.0 °C |
0.0324 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 50 Mobilube XFD Mobilube XFD 50 and 60 are extra high performance drivetrain lubricants engineered specifically to provide optimum component life when used as recommended in Caterpillar final drives and axles. Th.. |
|||
Density | 0.897 g/cc | 0.0324 lb/in³ | ISO 1183 |
ExxonMobil Exxtral™ LNV 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with high gloss, low warpage, and low discoloration in contact with hot water/steam in large electrical appliance such as washing mach.. |
|||
Density | 0.896 g/cc @Temperature 15.6 °C |
0.0324 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Solvesso™ Aromatic 150 Aromatic Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |
|||
Density | 0.897 g/cc @Temperature 15.6 °C |
0.0324 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 120 Exxon Aviation Oil Aviation Oil 100, 120 and 20W-50 are non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxid.. |
|||
Density | 0.896 g/cc @Temperature 15.0 °C |
0.0324 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 50 1650 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |
|||
Density | 0.896 g/cc | 0.0324 lb/in³ | |
ConocoPhillips Hydroclear® El Mar® 40 Ashless Supreme Description: Conoco Hydroclear El Mar Ashless Supreme is a premium ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Supreme is speci.. |
|||
Density | 0.898 g/cc @Temperature 15.0 °C |
0.0324 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 50 Exxon XD-3 Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d.. |
|||
Density | 0.897 g/cc @Temperature 15.0 °C |
0.0324 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 50 Mobilube XFD Mobilube XFD 50 and 60 are extra high performance drivetrain lubricants engineered specifically to provide optimum component life when used as recommended in Caterpillar final drives and axles. Th.. |
|||
Density | 0.897 g/cc | 0.0324 lb/in³ | ASTM D792 |
Dow Engage® 8440 Polyolefin Elastomer Description: Engage® 8440 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It is an excellent thermoplastic elastomer .. |
|||
Density | 0.898 g/cc | 0.0324 lb/in³ | |
BASF Butanediol Divinyl Ether Formula: C8H14N2CAS: 3891-33-6Description Butanediol divinyl ether is a colorless to yellow liquid, with a characteristic odor. It is soluble in water and with many organic solvents. Synonyms: BDDV.. |
|||
Density | 0.898 g/cc | 0.0324 lb/in³ | |
BASF Butyl Acrylate Formula: C7H12O2CAS: 141-32-2Description: Acrylic acid ester, for manufacturing polymers and for use as a feedstock for syntheses.Applications: Butyl acrylate forms homopolymers and copolymers. Copo.. |
|||
Density | 0.896 g/cc | 0.0324 lb/in³ | |
ConocoPhillips Hydroclear® 2500 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |
|||
Density | 0.898 g/cc | 0.0324 lb/in³ | |
BASF Ethylenediamine (EDA) Formula: C2H8N2CAS: 107-15-3Description: Ethylenediamine (EDA) is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: EDA, 1,2-Ethanediamine, 1,2-Diamineoethane,.. |