Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2215 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance and flexibility, short open time, and good wettingApplications: Component of hot melt adhes.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2280 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance and flexibility, short open time, and high viscosityApplications: Component of hot melt adh.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2304 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Excellent flexibility, wetting characteristics, and medium open timeApplications: Component of hot melt adhesive.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2730 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point, medium viscosity, good track, and very long open timeApplications: Component of hot me.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2732 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point, medium viscosity, good tack, and very long open timeApplications: Component of hot mel.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 3180 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Propylene homopolymer and FDA compliantFeatures: Temperature resistance, high melt viscosity, and increased hardnessApplications: Component of modified bi.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 3385 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: High melt viscosity, balanced temperature resistance, and flexibilityApplications: Component of modified bit.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 4304 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Low melt viscosity, moisture barrier, and adhesionApplications: Flooding and filling compounds for wire and cableOther.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 4460 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance high temperature resistance and low temperature flexibilityApplications: Wire and Cable fillings and flooding .. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D792 |
Proto3000 CastForm™ PS Selective Laser Sintering (SLS®) Prototyping Polymer Description: Directly produce complex investment casting patterns without tooling..Features: Functions like foundry wax and is “foundry friendly”Low residual ash content (less than 0.02%)Short bur.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 1330 Amorphous Polyalphaolefin (APAO) Laminate Grade.Description: Ethylene copolymer and FDA compliantFeatures: Medium open timeApplications: Lamination of reinforced tapes and protective overwrapsOther Properties: Ring and Ball Softeni.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2115 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Propylene homopolymer and FDA compliantFeatures: High softening point and short open timeApplications: Component of hot melt adhesives, sealants and specialty.. |
|||
Density | 0.860 g/cc @Temperature 15.6 °C |
0.0311 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 150 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil 798 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D297 |
Dow Nordel® IP 3430 EPDM Hydrocarbon Rubber Description: This amorphous, very low diene containing ethylenepropylene terpolymer (EPDM) is suitable for peroxide cured articles. Nordel® IP 3430 can also be blended with butyl rubber to improve .. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D297 |
Dow Nordel® IP 3640 EPDM Hydrocarbon Rubber Description: This is an amorphous and low-diene containing ethylene-propylene terpolymer (EPDM) suitable for heat resistant peroxide cured moldings. NDR 3640.00 can be blended with butyl rubber to i.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D297 |
Dow Nordel® IP 4520 EPDM Hydrocarbon Rubber Description: Nordel® IP 4520 is an amorphous EPDM grade designed for molded applications. It is ideally suited for injection and transfer molded brake parts, corner moldings, general purpose gasket.. |
|||
Density | 0.862 g/cc | 0.0311 lb/in³ | |
ConocoPhillips 32 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
ConocoPhillips Hydroclear Diamond Class® 32 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D297-93 |
Dow Nordel® IP 5565 EPDM Hydrocarbon Rubber Description: Nordel® IP 5565 is an amorphous, high diene, EPDM grade designed for extruded applications requiring fast cure rates. It is ideally suited for continuously cured dense and sponge profi.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
ConocoPhillips Hydroclear® 32 Turbine Oil Description: Conoco Hydroclear Turbine Oil is a premium rust- and oxidationinhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Turbine Oil is specially formula.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
BASF 1,2-PDA 1,2-Propylenediamine Formula: C3H10N2CAS: 78-90-0Description: 1,2-Propylenediamine is a colorless liquid, with an amine-like odor. It is also miscible with water in all proportionsSynonyms: 1,2-PDA, 1,2-Propanediamine,.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | Sintered; ASTM D792 |
ALM PS 200 Prototyping Polymer Non-spherical polystyrene powder for production of complex investment casting patterns.PS-200 can be used as a direct drop in replacement for Castform®, and can be successfully blended with Castfor.. |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil 1 10W-30 Mobil 1 10W-30 is the most advanced performance synthetic engine oil designed to provide the cleaning power, wear protection and performance reserve to keep engines running smooth and clean. Mobil 1.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 3330 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance temperature resistance and flexibilityApplications: Component of modified bitumen roofing systemsOth.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 3585 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: High melt viscosity and excellent low temperature flexibilityApplications: Component of modified bitumen roo.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 5224 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: High molecular weight REXtac, high ethylene copolymer, and FDA compliantFeatures: High viscosity and low crystallinityApplications: Component of modified .. |
|||
Density | 0.860 g/cc @Temperature 20.0 °C |
0.0311 lb/in³ @Temperature 68.0 °F |
|
Unipetrol PND 33-352-94 Extra Light Fuel Oil Extra light fuel oil si a mix of liquid hydrocarbons obtained from crude oil through distillation and other refining processes, boiling mostly within 150 to 370 °C. It may contain additives to lowe.. |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil 798 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |
|||
Density | 0.862 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Velocite 10 The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra.. |