REXtac Rextac® RT 3385 Amorphous Polyalphaolefin (APAO)

Category Polymer , Thermoplastic , Polyalphaolefin , Polyolefin
Manufacturer REXtac
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF REXtac Rextac® RT 3385 Amorphous Polyalphaolefin (APAO).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: High melt viscosity, balanced temperature resistance, and flexibilityApplications: Component of modified bitumen roofing systemsOther Properties: Ring and Ball Softening Point (ASTM E 28): 141°C.Needle Penetration (ASTM D 1321): 20 mm.Melt Density (190°C; Huntsman Method): 0.74 g/cc.Flashpoint, COC (ASTM D 93): >235°C.Information provided by Huntsman Corporation.
Physical Properties Metric English Comments
Density 0.860 g/cc
0.0311 lb/in³
ASTM D 792
Viscosity 8500 cP

@Temperature 190 °C
8500 cP

@Temperature 374 °F
melt viscosity; ASTM D 3236
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Flexibility Fail Temperature; Huntsman Method
Glass Transition Temp, Tg -29.0 °C
-20.2 °F
ASTM D3417