Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.780 - 3.20 g/cc | 0.0282 - 0.116 lb/in³ | Average value: 1.21 g/cc Grade Count:77 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Density | 0.780 - 0.830 g/cc | 0.0282 - 0.0300 lb/in³ | ASTM D4052 |
ExxonMobil Jayflex™ 220 Aliphatic Hydrocarbon Plasticizer Availability: North AmericaCAS Number: 64742-47-8Information provided by ExxonMobil |
|||
Density | 0.780 - 0.820 g/cc | 0.0282 - 0.0296 lb/in³ | ASTM D4052 |
ExxonMobil Pentamer CAS Number: 68514-35-2EC Number: 271-036-4Information provided by ExxonMobil |
|||
Density | 0.781 g/cc @Temperature 15.6 °C |
0.0282 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Varsol™ 18 Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: North America and South AmericaInformation provided by ExxonMobil |
|||
Density | 0.780 g/cc | 0.0282 lb/in³ | |
BASF Tributylamine Formula: C12H27NCAS: 102-82-9Description: Tributylamine is a colorless liquid with an amine-like odor. Synonyms: Tri-n-butylamine, 1-Butanamine,N,N-dibutyl, N,N-Dibutylbutan-1-aminApplications: Inte.. |
|||
Density | 0.780 g/cc | 0.0282 lb/in³ | |
LATI Latimass 47/7-04 D008 PP Copolymer Specific density compound based on Polypropylene copolymer (PPc). Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In.. |
|||
Density | 0.780 g/cc | 0.0282 lb/in³ | |
LATI Latimass 53-04 D008 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Density | 0.780 - 2.80 g/cc | 0.0282 - 0.101 lb/in³ | Average value: 0.928 g/cc Grade Count:188 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Density | 0.780 - 2.77 g/cc | 0.0282 - 0.100 lb/in³ | Average value: 0.952 g/cc Grade Count:729 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |