Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.700 g/cc | 0.0253 lb/in³ | Average Density |
Potters Industries Conduct-O-Fil® AGSF-20 Silver-coated Hollow Ceramic Spheres Applications: Conductive paints and coatings; Aerospace and other mass-critical applications. Advantages include low density, easily mixed into paint systems, large particle sizeInformation provide.. |
|||
Density | 0.700 - 1.20 g/cc | 0.0253 - 0.0434 lb/in³ | Average value: 1.17 g/cc Grade Count:249 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Density | 0.700 - 1.56 g/cc | 0.0253 - 0.0564 lb/in³ | Average value: 1.43 g/cc Grade Count:19 |
Overview of materials for Chlorinated PVC (CPVC) This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 0.700 - 3.35 g/cc | 0.0253 - 0.121 lb/in³ | Average value: 2.07 g/cc Grade Count:103 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |
|||
Density | >= 0.700 g/cc @Temperature 20.0 °C |
>= 0.0253 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-15 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | 0.700 - 1.10 g/cc | 0.0253 - 0.0397 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 847.6 Agglomerated Yttria (Y2O3) |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | |
Synergy Polymers Ultra Purge HIGH-E Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents to help in clean.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | |
Synergy Polymers Ultra Purge P-O Ultra Purge is a specially designed cleaning compound that comes premixed and ready-to-use in pellet form. It cleans black specks and deposits from screws, barrels, nozzle, hot runners and heads of .. |
|||
Density | <= 0.700 g/cc @Temperature 0.850 °C |
<= 0.0253 lb/in³ @Temperature 33.5 °F |
|
Solvay Chemicals CASO® Granular Anhydrous Calcium Chloride CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10043-52-4/ EINECS - .. |
|||
Density | <= 0.700 g/cc @Temperature 0.850 °C |
<= 0.0253 lb/in³ @Temperature 33.5 °F |
|
Solvay Chemicals CASO® Granular Anhydrous Calcium Chloride >94% CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10043-52-4/ EINECS - .. |
|||
Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Shandong Dongyue Polymer DF-31A PTFE Pelletized Resin Usage: The resin is used to auto press molding and ram extrusion all kinds of rods, pipe etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF.. |
|||
Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Shandong Dongyue Polymer DF-31B PTFE Pelletized Resin Usage: The resin is used to auto press molding and ram extrusion all kinds of rods, pipe etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF.. |
|||
Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ 350 Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ CG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ FM-1 Hollow Spheres EXTENDOSPHERESâ„¢FM-1 ceramic hollow spheres are a low-density functional additive for disc brake pads, truck and train blocks, clutch facings and other friction materials. They are compatible wi.. |
|||
Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ MG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Density | 0.700 - 0.800 g/cc | 0.0253 - 0.0289 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ SG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
Sinotek Materials B Graphite Roll Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
Sinotek Materials B Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | ISO 1183 |
Borealis Borcoat™ GA700E-7032 Syntactic Polypropylene for Steel Pipe Coating Borcoat GA700E-7032 is a grey colored syntactic, high impact polypropylene with high thermal insulation capacity and high compressive strength.Borcoat GA700E-7032 is recommended as thermal insulatio.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | Calculated number using basis weight and thickness |
DuPont™ Nomex® Type 993, 40 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | Apparent; ASTM D1182 |
Chi Mei Acryrex® CM-205 PMMA High heat injection grade. It can resist high temperature. High mechanical strength.Applications: The indicator cover of scooter and automobile/sun glasses/digital watch cover.Features:Good Weather .. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | Apparent; ASTM D1182 |
Chi Mei Acryrex® CM-207 PMMA Features:General PurposeGood Weather ResistanceHigh GlossHigh Heat ResistanceHigh StrengthMedium ViscosityUses: Automotive Interior PartsBathroom AccessoriesContainersCosmeticsHousehold GoodsKnobsRo.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | Apparent; ASTM D1182 |
Chi Mei Acryrex® CM-211 PMMA Features:Good Weather ResistanceHigh ClarityHigh FlowHigh GlossHigh Heat ResistanceHigh ViscosityUses:ContainersCosmeticsHousehold GoodsKnobsRoHS CompliantAppearance: Clear/TransparentForms: Pellets.. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | |
Arkema Group Lucalor® RB 8067 CPVC, Pipe Grade LUCALOR RB 8067 is the trade name for CPVC made by Elf Atochem. It is manufactured with a patented mass PVC resin chlorination process.* MAIN CHARACTERISTICS Chlorine content:67.0%. Viscosity index .. |
|||
Density | 0.700 g/cc | 0.0253 lb/in³ | ASTM C134 |
BNZ Materials BNZP-23B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
Sinotek Materials A Graphite Roll Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.06 |
Sinotek Materials C Graphite Roll Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.06 |
Sinotek Materials C Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.07 |
Sinotek Materials D Graphite Roll Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |