Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.480 g/cc | 0.0173 lb/in³ | Geon® 1169; Internal Method |
PolyOne Syncure™ S1010B Polyethylene, Crosslinked (XLPE) Available as Catalyst Masterbatch component for PolyOne Syncure System.Oven Aging values are >75, and were measured on a 95 phr S1025A / 5 phr S1010B Syncure System. Pellet appearance is 1/8 cylindr.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | Effective density of spheres |
Potters Industries Q-Cel® 6048 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Density | 0.480 - 0.640 g/cc | 0.0173 - 0.0231 lb/in³ | |
Pyrotek PTB 2200 Structural Board ApplicationsCaster tips Small machined nozzles Slotted caster tips AdvantagesHigh strength Resistant to thermal shock Easily machined Non-wetting to molten non-ferrous metals Low thermal mass High t.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | |
Pyrotek Wollite 30 Insulating Castable Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting c.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | Geon® 1169; Internal Method |
PolyOne Syncure™ S1017B Polyethylene, Crosslinked (XLPE) Available as Catalyst Masterbatch component for PolyOne Syncure System.Oven Aging values are >75, and were measured on a 98.5 phr S1025A / 1.5 phr S1017B Syncure System. Torque is >1500. Pellet appe.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | ASTM D3574A |
Mearthane Durethaneâ„¢ F DF-630A Closed Cell Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 75Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | ASTM D3574A |
Mearthane Durethaneâ„¢ M DM-630A Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 75Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | ASTM D3574A |
Mearthane Durethaneâ„¢ M DM-720A Foam Polyurethane MDI backbone: ether.Shore 00 Hardness: 65Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
Density | 0.480 - 0.670 g/cc | 0.0173 - 0.0242 lb/in³ | Free flowing, Specification |
Solvay Chemicals Soda Solvay® Light Soda Ash (European Grade) Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | |
Sawbones Solid Rigid Polyurethane Foam 30 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | Expanded Compound; ASTM D792 |
Borealis Borcell™ HE1344 High Density Polyethylene Compound for Cellular Insulation of Data Cables Borcell HE1344 is a high-molecular weight, high-density polyethylene (HDPE) insulation compound containing an industry approved non plate-out chemical blowing agent. It contains the required levels.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | |
Zircar Ceramics AL-30 Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | |
Zircar Ceramics SALI Alumina Insulation SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength.Information provi.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | ASTM D792 |
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 30 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | |
3M Cushion-Mount™ E1715 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Density | 0.480 - 0.520 g/cc | 0.0173 - 0.0188 lb/in³ | True, 3M QCM 14.24.6 |
3M H50/10000EPX Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | |
3M Cushion-Mount™ 1720M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | |
3M Cushion-Mount™ E1720 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Density | 0.480 g/cc | 0.0173 lb/in³ | |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |