Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.210 g/cc | 0.00759 lb/in³ | Effective density of spheres |
Potters Industries Q-Cel® 300 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Density | 0.210 g/cc | 0.00759 lb/in³ | |
Pyrotek Fiberseal Paper C-6 Ceramic fiber paper C-6 is an economical, high strength, Fiberseal paper composed of ceramic fibers, inert fillers and fiberglass.ApplicationsGaskets Seals Linings AdvantagesLow shrinkage Good dielectric properties Uni.. |
|||
Density | 0.210 g/cc | 0.00759 lb/in³ | Pour Density; ASTM D1513 |
TIMCAL ENSACO™ 210G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Density | 0.210 - 0.250 g/cc | 0.00759 - 0.00903 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 446 NDN NR-SBR Foam Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.210 - 0.290 g/cc | 0.00759 - 0.0105 lb/in³ | ISO 845-88 |
Eurofoam Siliconcell SIL 411 Silicone Foam Sheet Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |
|||
Density | 0.210 - 0.230 g/cc | 0.00759 - 0.00831 lb/in³ | Free Density |
C.O.I.M. UREXTER® F 3 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Density | 0.210 g/cc | 0.00759 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® T90.210 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has good mechanical properties and resistance to fatigue, is chemic.. |
|||
Density | 0.210 g/cc | 0.00759 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |
|||
Density | 0.210 g/cc | 0.00759 lb/in³ | |
Pyrotek M-12 Compressible/Insulating Boards ApplicationsHigh temperature gaskets Furnace covers Trough lining AdvantagesLow density Good insulating ability Information provided by Pyrotek. |
|||
Density | 0.210 - 1.50 g/cc | 0.00759 - 0.0542 lb/in³ | Average value: 1.17 g/cc Grade Count:125 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |