Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.152 - 0.208 g/cc | 0.00550 - 0.00752 lb/in³ | Dry |
Reade Advanced Materials Diatomaceous Earth (DE) (SiO2·nH2O) Description: A naturally occurring mineral derived from microscopic in size fossilized remains of marine diatoms. It has high absorption, low bulk density and high brightness.A silica source in the .. |
|||
Density | 0.152 g/cc | 0.00550 lb/in³ | ASTM D1056 |
Rogers Corporation Bisco® MF1 9575 - 75 Silicone, High Performance Foam, Indentation Force Material MF1® 9575 is a high quality silicone foam material designed for a wide range of cushioning and sealing applications. It features exceptional flame, smoke and toxicity (FST) characteristics, superi.. |
|||
Density | 0.152 g/cc | 0.00550 lb/in³ | ASTM D1056 |
ACC Magnifoam™ MF1-9575™ MTI Silicones Silicone Foam Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Density | 0.152 g/cc | 0.00550 lb/in³ | Nominal Core Density |
Unifrax Fiberfrax® Duraset® Flet Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers i.. |