Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0600 g/cc | 0.00217 lb/in³ | apparent nominal; ISO 845 |
3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam AIREX® C51 is a closed-cell polymer foam with outstanding damage tolerance and formability. Its excellent price / performance ratio uniquely qualifies this core material for high-volume sandwich .. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | 2.5 minute residence time pre-expander |
Jackon JACKOCELL® S232 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S232 which will lead the industry in.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | ASTM D1622 |
SABIC Innovative Plastics ULTEM Foam XP060 PEI ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The .. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® HD60 High Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® LD60 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0600 - 0.0760 g/cc | 0.00217 - 0.00275 lb/in³ | sheet density |
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0600 - 0.100 g/cc | 0.00217 - 0.00361 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-S EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | ISO 845 |
BASF Neopolen® P 9035 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | ISO 845 |
BASF Neopolen® P 9225 K 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | ISO 845 |
BASF Neopolen® P 9230 A 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | ISO 845 |
BASF Neopolen® P 9230 D 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | ISO 845 |
BASF Neopolen® P 9335 MG 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | ISO 845 |
BASF Neopolen® P 9435 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with high damage tolerance. This one of a kind formula combines very high elongation and excellent bond strength. AIREX® R63 is cold.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Density | 0.0600 - 0.0700 g/cc | 0.00217 - 0.00253 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | ISO 845 |
BASF Neopolen® P 9230 K 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | ISO 845 |
BASF Neopolen® P 9235 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | ISO 845 |
BASF Neopolen® P 9255 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® C70.55 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Density | 0.0600 g/cc | 0.00217 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |
|||
Density | 0.0600 - 1.69 g/cc | 0.00217 - 0.0611 lb/in³ | Average value: 1.37 g/cc Grade Count:812 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |