Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0330 g/cc | 0.00119 lb/in³ | 0.5 minute residence time pre-expander |
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |
|||
Density | 0.0330 g/cc | 0.00119 lb/in³ | 0.5 minute residence time pre-expander |
Jackon JACKOCELL® R411 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThe unique design of polystyrene chains and additive chemistry in the Jackocell® R411 gives pre-expanded beads of high dimensional stability. The R411 represents the.. |
|||
Density | 0.0330 g/cc | 0.00119 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0330 g/cc | 0.00119 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® LD33FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0330 g/cc | 0.00119 lb/in³ | ISO 845 |
Zotefoams ZOTEK® F OSU Flexible PVDF Foam Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and .. |
|||
Density | 0.0330 g/cc | 0.00119 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® LD33LC Low Density Polyethylene Foam, Large Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0330 g/cc | 0.00119 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® MP33 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0330 g/cc | 0.00119 lb/in³ | ISO 845 |
Zotefoams ZOTEK® F 35 PVDF Foam Zotek® F 35 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Density | 0.0330 g/cc | 0.00119 lb/in³ | Free Rise Density (Cured) |
Dow BETAFOAM™ 87100/87120 BETAFOAM™ 87100/87120 is a low density, all water blown rigid polyurethane foam. These components were engineered to produce a foam for providing barrier protection against airborne noise. Foam i.. |
|||
Density | 0.0330 - 0.0390 g/cc | 0.00119 - 0.00141 lb/in³ | |
Akzo Nobel Expancel® 461 WE 20 d36 Wet expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0330 - 0.0390 g/cc | 0.00119 - 0.00141 lb/in³ | |
Akzo Nobel Expancel® 551 WE 40 d36 Wet expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0330 - 0.0390 g/cc | 0.00119 - 0.00141 lb/in³ | |
Akzo Nobel Expancel® 551 WE 80 d36 Wet expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0330 g/cc | 0.00119 lb/in³ | |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |