Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.0300 g/cc | >= 0.00108 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 340R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0300 - 0.100 g/cc | 0.00108 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 340R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | >= 0.0300 g/cc | >= 0.00108 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 350R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0300 - 0.100 g/cc | 0.00108 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 350R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | 0.6 minute residence time |
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ PM 6550 Hollow Plastic Spheres PM 6550 PM 6550 is an extremely light and versatile hollow sphere. Its plastic composition results in a very low density product. Only a very small amount of this hollow sphere is needed to provide .. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Evazote® EV30 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® HD30 High Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0300 - 0.0390 g/cc | 0.00108 - 0.00141 lb/in³ | sheet density |
Zotefoams Plastazote® HL34 Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | ISO 845 |
Zotefoams ZOTEK® F 30 PVDF Foam Zotek® F 30 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Density | <= 0.0300 g/cc | <= 0.00108 lb/in³ | TMA |
Akzo Nobel Expancel® 461 DU 20 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0300 g/cc | <= 0.00108 lb/in³ | TMA |
Akzo Nobel Expancel® 461 WU 20 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | ISO 845 |
BASF Neopolen® P 8220 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | ISO 845 |
BASF Neopolen® P 8225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | |
BASF E-por® 0.03 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | ISO 845 |
BASF Neopolen® P 9225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | ISO 845 |
BASF Neopolen® P 8015 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Density | 0.0300 g/cc | 0.00108 lb/in³ | |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Density | >= 0.0300 g/cc | >= 0.00108 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
Ineos Nova W441A Expandable Polystyrene A regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for high density foam applications.Applications: This grade is sued mainly for.. |
|||
Density | 0.0300 - 0.0800 g/cc | 0.00108 - 0.00289 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
Ineos Nova W441A Expandable Polystyrene A regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for high density foam applications.Applications: This grade is sued mainly for.. |
|||
Density | >= 0.0300 g/cc | >= 0.00108 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Styrocell® D933A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic.. |