Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.86 - 3.94 g/cc | 0.139 - 0.142 lb/in³ | Sintered |
Nabaltec GRANALOX® NM 9915 B Ceramic Body, Binder Free Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti.. |