Physical Properties Metric English Comments
Density 0.780 - 3.20 g/cc
0.0282 - 0.116 lb/in³
Average value: 1.21 g/cc Grade Count:77
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Density 2.50 - 3.20 g/cc
0.0903 - 0.116 lb/in³
ASTM B417
H.C. Starck Amperit® 584.072 Chromium Carbide-Nickel-Chromium 75-25 (Cr3C2-NiCr)
Density 2.50 - 3.20 g/cc
0.0903 - 0.116 lb/in³
ASTM B417
H.C. Starck Amperit® 588.059 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr)
Density 2.60 - 3.20 g/cc
0.0939 - 0.116 lb/in³
ASTM B212
H.C. Starck Amperit® 599.074 Agglomerated Sintered Molybdenum Carbide (Cr2O3)
Density 2.60 - 3.20 g/cc
0.0939 - 0.116 lb/in³
Goodfellow Potassium Aluminosilicate (Muscovite Mica)
Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin..