Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.15 - 2.25 g/cc
0.0777 - 0.0813 lb/in³
ASTM D792
Polikim EFALON® C-15 PTFE, 15% Glass Filled
C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings..
Density 1.15 - 2.25 g/cc
0.0415 - 0.0813 lb/in³
Average value: 1.47 g/cc Grade Count:33
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
Density 2.23 - 2.25 g/cc
0.0806 - 0.0813 lb/in³
molded; ASTM D792
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber
PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re..