Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.940 - 0.956 g/cc | 0.0340 - 0.0345 lb/in³ | Average value: 0.950 g/cc Grade Count:8 |
Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Carbon Black Filled". Each property range of values reported is minimu.. |
|||
Density | 0.952 - 0.956 g/cc | 0.0344 - 0.0345 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HD 7255 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.952 - 0.956 g/cc | 0.0344 - 0.0345 lb/in³ | DIN 53479 |
Iran Petrochemical (PCC) Arak I4 HDPE Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.952 - 0.956 g/cc | 0.0344 - 0.0345 lb/in³ | DIN 53479 |
Iran Petrochemical (PCC) Arak BL3 HDPE Information provided by Iran Petrochemical Commercial Co. |