Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.919 - 0.921 g/cc | 0.0332 - 0.0333 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) Arak 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.919 - 0.921 g/cc | 0.0332 - 0.0333 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) Arak 20075AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.919 - 0.921 g/cc | 0.0332 - 0.0333 lb/in³ | ASTM D792 |
Iran Petrochemical (PCC) Tabriz 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.917 - 0.921 g/cc | 0.0331 - 0.0333 lb/in³ | |
Kazanorgsintez 15813-020 High Pressure Polyethylene Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac.. |