Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.857 - 0.913 g/cc | 0.0310 - 0.0330 lb/in³ | ASTM D792 |
Dow Engage® Polyolefin Elastomer Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. .. |
|||
Density | 0.849 - 0.913 g/cc | 0.0307 - 0.0330 lb/in³ | |
CMT Materials HYTAC® WF High Strength High Clarity 450°F Epoxy Syntactic HYTAC-WF is an excellent high temperature epoxy syntactic material that provides improved clarity when forming APET and other clear polymers plus reduces sticking of difficult to process polymers su.. |
|||
Density | 0.833 - 0.913 g/cc | 0.0301 - 0.0330 lb/in³ | Average value: 0.847 g/cc Grade Count:12 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |