Polymer Property : Density = 0.150 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.120 - 0.150 g/cc
0.00434 - 0.00542 lb/in³
typical range; ISO 845
3A Composites Core Materials AIREX® C70.130 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli..
Density 0.100 - 0.150 g/cc
0.00361 - 0.00542 lb/in³
Sharadaa Ceramics Resin Bonded Mattresses
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Density 0.110 - 0.150 g/cc
0.00397 - 0.00542 lb/in³
ISO 845-88
Eurofoam Porocell POR 304 B EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.