Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.22 g/cc | 0.333 lb/in³ | |
Indium Corp. Indalloy 76 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | at RT |
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | at RT |
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | at RT |
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | at RT |
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | at RT |
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | at RT |
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | at RT |
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | at RT |
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | |
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | |
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | |
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | |
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | |
ATI Allvac® Nickelvac® L-605 Cobalt-Nickel Superalloy, Heat Treatment: 1204°C (2200°F) Anneal Data provided by Allvac.Applications: High temperature applications, jet engine components, devices in high fatigue service. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | at RT |
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |
|||
Density | 9.22 g/cc | 0.333 lb/in³ | |
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |