Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.58 g/cc | 0.310 lb/in³ | |
Performance Alloys MoldStar® 90 Copper Mold Alloy Description: MoldStar® 90 is a beryllium-free copper alloy for the blow molding and injection molding industries as well as other industrial applications. MoldStar® 90 provides a good balance of t.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | P/M (98%) |
Kennametal Stellite Stellite® STAR cast Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | P/M (98%) |
Kennametal Stellite Stellite® STAR with P/M Processing Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
Indium Corp. Indalloy 69 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
Indium Corp. Indalloy 75 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
H.C. Starck Grain Stabilized Niobium (GSNb) GSNb is a patent pending single-phase micro-alloy that has a grain size of approximately 2 ASTM numbers finer than standard commercial grade niobium.Applications: Grain Stabilized Niobium (GSNb) is.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
LATI Latigray 82-03 CW/95 PA 12, Metallic Reinforced Radiopaque compound based on Polyamide 12 (PA12). Metallic filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, 1/2 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, 1/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, 3/4 Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, Annealed 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, Extra Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, Extra Spring 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | Annealed |
Eagle Brass 762 Nickel Silver 12%, Spring 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C27450 Copper-Zinc Alloy Finished product available as wire or tube.Chicago Extruded Metal temper code: H04Information provided by Chicago Extruded Metals |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
ATI Wah Chang Nb/Nb Alloy Nb-I ZR Improved creep strength versus pure niobium. Replacement for pure niobium in applications requiring the chemical resistance of niobium and a material with high melting temperature.Information provid.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
AIM 58 Fusible Alloy Uses: lens blocking; proof casting; fusible element in safety devices; anchoring parts for machining; sealing adjustment screws; holding jet engine blades for machining and broaching; filler for sup.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
ATI Wah Chang Niobium Niobium is a soft, ductile metal which can be cold worked over 90 percent before annealing becomes necessary. In appearance, the metal is somewhat similar to stainless steel. The density of 8.57 gm/.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
Wall Colmonoy COLMONOY® 22 - Nickel Alloy With Tungsten Carbide Description and Application: A harder version of Colmonoy 23A and 24, for similar applications. Can be finished with a file.Method of Application: Oxyacetylene, FusewelderInformation provided by Wa.. |
|||
Density | 8.58 g/cc | 0.310 lb/in³ | |
Wall Colmonoy COLMONOY® 226 - Custom Formulated Nickel-Based Alloy For Glass Patented alloy specially designed for glass container mold protection and restoration. Also used for rebuilding automotive parts (clutch components).Method of Application: FusewelderInformation pro.. |