Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.17 g/cc | 0.295 lb/in³ | |
IBC Advanced Alloys 42C Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |
|||
Density | 8.17 g/cc | 0.295 lb/in³ | |
Latrobe Crusaderâ„¢ ASTM M3-2 High Speed Steel CRUSADER (M3-2) is a high speed steel with an outstanding balance of red hardness, edge toughness and wear resistance. The additional carbon and vanadium provide good resistance to abrasion and edge.. |
|||
Density | 8.17 g/cc | 0.295 lb/in³ | theoretical |
Kennametal Stellite Deloro® 716 PM cast Adhesive wear test data: cast 0.1; abrasive wear test data: cast 63 mm^3. Deloro 716 is currently being developed. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball .. |
|||
Density | 8.17 g/cc | 0.295 lb/in³ | theoretical |
Kennametal Stellite Deloro® 716 PM with P/M Processing Adhesive wear test data: cast 0.1; abrasive wear test data: cast 63 mm^3. Deloro 716 is currently being developed. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball .. |
|||
Density | 8.17 g/cc | 0.295 lb/in³ | |
Latrobe Corsairâ„¢ ASTM M3-1 High Speed Steel CORSAIR (M3-1) contains carbon and vanadium levels that are intermediate between those of Double Six (M2) and Crusader (M3-2). This gives the steel a fine balance of wear
resistance and grindability.. |
|||
Density | 8.17 g/cc | 0.295 lb/in³ | |
Special Metals INCOLOY® alloy 908 INCOLOY® alloy 908 (UNS N09908) is an age-hardenable nickel-iron alloy which exhibits a low coefficient of thermal expansion, high tensile strength, high fracture and impact toughness, fatigue cr.. |
|||
Density | 8.17 g/cc | 0.295 lb/in³ | |
Williams Advanced Alloys WS186 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 8.17 g/cc | 0.295 lb/in³ | |
Crucible Steel CPM® Rex® 20® (HS) High Speed Steel CPM Rex 20 is a cobalt-free super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has heat treat response and red hardness comparable to that of M42 but offers better wea.. |
|||
Density | 8.17 g/cc | 0.295 lb/in³ | |
Crucible Steel REX® M3-1 High Speed Steel, AISI M3-1 REX M3-1 is a lower carbon, lower vanadium modification of M3-2 high speed steel. This lower alloy content results in better machining and grinding characteristics compared to M3-2, with a slight im.. |
|||
Density | 8.17 g/cc | 0.295 lb/in³ | |
California Fine Wire Manganin 230 (Shunt) Copper, Manganese, and Nickel Resistance Wire All values may vary dependent on specific design and usageNickel content modifiedCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.17 g/cc | 0.295 lb/in³ | |
ATI Allegheny Ludlum AL 4750™ Electrical Alloy, UNS K94800 or UNS K95000 The alloy produces good magnetic properties, wide latitude to control hysteresis loop shape via recrystallization modes. Applications for this grade range from electromechanical relay cores, to ver.. |