Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.97 g/cc | 0.288 lb/in³ | |
Latrobe Starkâ„¢ ASTM M4 High Speed Steel STARK (M4) is a super high speed steel with very high carbon and vanadium contents for exceptional abrasion resistance. It is well suited for premium cutting tools of all types,
particularly those u.. |
|||
Density | 7.97 g/cc | 0.288 lb/in³ | |
Crucible Steel CPM® Rex M4 HC(HS) Tool Steel CPM REX M4 HC(HS) is a high vanadium special purpose high speed steel exhibiting better wear resistance and toughness than M2 or M3 in cold work punches, die inserts and cutting applications involvi.. |
|||
Density | 7.97 g/cc | 0.288 lb/in³ | |
Crucible Steel HALCOMB® 425 Tool Steel, AISI H19 Halcomb 425 is designed for higher operating temperatures than H13, where wear resistance and heat check resistance are more critical than toughness. While H19 has excellent heat checking resistance.. |
|||
Density | 7.97 g/cc | 0.288 lb/in³ | |
Carlson 330 Austenitic Alloy General DescriptionCarlson Alloy 330 is a nickel-iron-chromium-silicon austenitic alloy. It combines high strength with excellent resistance to carburization and oxidation at temperatures to 2200°.. |
|||
Density | 7.97 g/cc | 0.288 lb/in³ | |
Carlson 904L Austenitic Stainless Steel General Description904L is an austenitic nickel-chromium stainless steel with molybdenum and copper additions. The elevated nickel and chromium content of 904L make it resistant to corrosion in a w.. |
|||
Density | 7.97 g/cc | 0.288 lb/in³ | |
Carpenter Four Star High Speed Steel Red-Wear® (AISI M4) Carpenter Four Star, a molybdenum-tungsten high speed tool steel possessing high carbon and vanadium contents, provides a very high degree of wear resistance coupled with high strength.Applications:.. |
|||
Density | 7.97 g/cc | 0.288 lb/in³ | |
Carpenter AerMet® 310 AerMet 310 alloy possesses higher hardness and strength than AerMet 100 alloy while maintaining exceptional ductility and toughness. At a 310 ksi (2137 MPa) ultimate tensile strength, AerMet 310 all.. |