Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.64 g/cc | 0.276 lb/in³ | |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
Schmolz + Bickenbach 416RS Stainless Steel Bar Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
Crucible Steel 430F Stainless Steel Crucible 430F is a low carbon, high chromium ferritic stainless steel, specially developed for solenoid core applications in corrosive environments. The chemistry is closely controlled to develop o.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
Crucible Steel 440C Chromium Steel Crucible 440C is a hardenable chromium steel. It has one of the highest attainable hardnesses of the corrosion and heat resisting grades. This grade is magnetic at all times.Information provided b.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
Crucible Steel CSM® 420 XL Stainless Steel CSM 420 XL is the workhorse premium quality stainless mold steel designed for applications requiring a combination of corrosion resistance and wear resistance. It is double melted for the microstruc.. |
|||
Density | 7.64 g/cc @Temperature 199 °C |
0.276 lb/in³ @Temperature 390 °F |
hardened to 62 HRC |
Bohler-Uddeholm AISI D2 Cold Work Tool Steel AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadiumAISI AD2 is characterized by: High wear resistance High compressive strength Good through-hardening properties.. |
|||
Density | 7.64 g/cc @Temperature 200 °C |
0.276 lb/in³ @Temperature 392 °F |
|
Assab Steels ASSAB XW-41 Cold Work Steel XW-41 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength Good through-hardening propertiesHigh stability i.. |
|||
Density | 7.64 g/cc @Temperature 200 °C |
0.276 lb/in³ @Temperature 392 °F |
|
Assab Steels ASSAB XW-42 Cold Work Steel XW-42 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength High hardness after hardeningGood through-hardeni.. |
|||
Density | 7.64 g/cc @Temperature 200 °C |
0.276 lb/in³ @Temperature 392 °F |
|
Assab Steels ASSAB XW-5 Cold Work Steel ASSAB XW-5 is a high-carbon, high chromium tool steel alloyed with tungsten, characterized by:High wear resistanceHigh compressive strengthHigh surface hardness after hardeningGood through-hardening.. |
|||
Density | 7.64 g/cc @Temperature 400 °C |
0.276 lb/in³ @Temperature 752 °F |
|
Assab Steels CALMAX Plastic Mold Material CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum 410 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Relay Steels No. 5 Silicon and iron alloyApplications:relays, armatures, solenoids, magnetic clutches, pole pieces, certain types of motors, transformers, data processing equipment.Information provided by Allegheny Lu.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 593°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 649°C (1200°F) (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 760°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 538°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Density | 7.64 g/cc | 0.276 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |