Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.40 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy® 241 95.5Sn/3.8Ag/0.7Cu Lead-Free Solder Alloy Multicore promoted alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy® 246 95.5Sn/4.0Ag/0.5Cu Lead-Free Solder Alloy Petzow (German) prior art reference makes this alloy patent-free.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy® 252 95.5Sn/3.9Ag/0.6Cu Lead-Free Solder Alloy Alloy of choice for general SMT assembly. NEMI promoted alloy (average composition of Indalloy #241& #246).Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy Referred to as the SAC305 alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Sinotek Materials Tungsten Disulfide (WS2) Powder, High-Purity Tungsten Disulfide powder mainly has applications in spraying, coating, carbon material, all sorts of grease, lubricating oil, friction materials and catalysts. Tungsten Disulfide has good resistan.. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Goodfellow Nickel/Iron/Silicon/Boron Alloy Metallic glass (glassy alloy) or amorphous metal. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow.Composition Notes: Si + B co.. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
American Elements Europium Oxide Nanopwder General DescriptionEU-MITE powders and dispersions are inorganic europium-oxide nanoparticles. EU-MITE-A products are uncoated and hydrophilic. EU-MITE-O products are coated with an organic silane (.. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Crucible Steel CPM® S90V® (420V®) Tool Steel CPM S90V is a unique tool steel made by the Crucible Particle Metallurgy process. It is a martensitic stainless steel with a high volume of vanadium carbides for exceptionally good wear resistance. .. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
BryCoat WS2 Tungsten Disulfide Coating WS2's unique, extensively modified lamellar composition of tungsten disulfide results in a high performance dry coating lubricant. A pressurized air application processes impinges a dry metallic co.. |
|||
Density | >= 7.40 g/cc | >= 0.267 lb/in³ | |
Channel Industries 5700 Lead Zirconate Titanate Piezoelectric Navy Type VICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exten.. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy 203 Indium Solder Alloy Information Provided by Indium Corporation |