Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.32 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 160 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.32 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 258 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.32 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 260 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.32 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy® 262 Tin-Copper Solder Alloy Information provided by the manufacturer, Indium Corporation of America. |
|||
Density | 7.32 g/cc | 0.264 lb/in³ | |
Goodfellow Iron 81/Boron 13.5/Silicon 3.5 Alloy Information provided by Goodfellow. |