Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.00 - 5.60 g/cc | 0.181 - 0.202 lb/in³ | ASTM B417 |
H.C. Starck Amperit® 519.059 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Density | 5.00 - 5.60 g/cc | 0.181 - 0.202 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 519.074 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Density | 5.00 - 5.60 g/cc | 0.181 - 0.202 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 519.088 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Density | 5.00 g/cc | 0.181 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 527.074 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Density | 5.00 g/cc | 0.181 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 527.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Density | 5.00 g/cc | 0.181 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton 922 Yttria Y2O3 REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Density | 5.00 g/cc | 0.181 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp MH0500A PP (Asia Pacific) LNP THERMOCOMP* MH0500A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 5.00 g/cc | 0.181 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp MH0500A PP (Asia Pacific) LNP THERMOCOMP* MH0500A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 5.00 g/cc | 0.181 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp WH0500B PBT LNP* THERMOCOMP* WH0500B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was .. |
|||
Density | 5.00 g/cc | 0.181 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp WH0500B PBT (Asia Pacific) LNP* THERMOCOMP* WH0500B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was .. |
|||
Density | 5.00 g/cc | 0.181 lb/in³ | |
BASF Paliotan® Yellow L 1945 Color Additive Description: Pigment combination based on Bismuth VanadatSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Amine curing system and Airdrying systems.Information provided b.. |
|||
Density | 5.00 g/cc | 0.181 lb/in³ | |
Ceradyne Ceralloy® 398J Yttrium Oxide Ceralloy® 398J Hot Pressed Yttrium Oxide is a high purity hot-pressed ceramic exhibiting excellent corrosion and erosion resistance. Products produced from Hot Pressed Yttrium Oxide are for semicon.. |