Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.65 g/cc | 0.168 lb/in³ | Typical |
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4984 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4984.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |
|||
Density | 4.65 g/cc | 0.168 lb/in³ | Typical |
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4987 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4987.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |
|||
Density | 4.65 g/cc | 0.168 lb/in³ | Typical |
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4986 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4986.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |
|||
Density | 4.65 g/cc | 0.168 lb/in³ | Typical |
TIMET TIMETAL® 17 Titanium Alloy (Ti-5Al-2Sn-4Mo-2Zr-6Mo); Aged Billet/Bar Features: High strength, deep hardenable forging alloy primarily for jet engines. Allows heat treatment to a variety of strength levels in sections up to 6 inches. Offers good ductility and toughnes.. |
|||
Density | 4.65 g/cc | 0.168 lb/in³ | |
ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age Data provided by Allvac.Applications: Intermediate-temperature jet engine applications. Blades, discs, spacers, seals. Standard, rotor/premium grades. |
|||
Density | 4.65 g/cc | 0.168 lb/in³ | |
ATI Allvac® Ti-17 Titanium Alloy, Heat Treatment: 899°C (1650°F) + Age Data provided by Allvac.Applications: Compressor discs, heavy section forgings for gas turbine engine components. High tensile strength and good fracture toughness. |