Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.98 g/cc | 0.144 lb/in³ | |
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam.. |
|||
Density | 3.98 g/cc | 0.144 lb/in³ | |
Zircar Ceramics HC Sapphire (Single Crystal Aluminum Oxide) Hangar Clip ZIRCAR hanger clips are comprised of sapphire (single crystal aluminum oxide) and are designed for use with hanger rod (HR-1). The single crystal structure of these clips prevents creep and deformat.. |
|||
Density | 3.98 g/cc | 0.144 lb/in³ | |
Goodfellow Ruby, Al2O3 Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro.. |
|||
Density | 3.98 g/cc | 0.144 lb/in³ | |
Anderman Ceramics EA999 Sintered Alumina, 99.9% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Density | 3.98 g/cc | 0.144 lb/in³ | |
Mateck Sapphire (Al2O3) Optical crystals |
|||
Density | 3.98 g/cc | 0.144 lb/in³ | |
Mateck Sapphire Aluminium oxide Substrate, Al2O3 Substrate single crystals for superconductivity. |