Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.83 g/cc | 0.138 lb/in³ | DIN EN 623-2 |
CeramTec B 601 Alumina, 98.5% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |