Density 21.5 g/cc
0.777 lb/in³
Johnson Matthey SW 850 Platinum w/ 15% Iridium Jewelry Alloy
Springs, watch backs. Copper, cobalt, gold, iridium, palladium and ruthenium alloy easily with platinum. The differences between the alloys reflect the hardening of the alloying element itself.
Density 21.5 g/cc
0.777 lb/in³
Johnson Matthey SW 900 Platinum w/ 10% Iridium Jewelry Alloy
Safety catches, pins. Copper, cobalt, gold, iridium, palladium and ruthenium alloy easily with platinum. The differences between the alloys reflect the hardening of the alloying element itself.
Density 21.5 g/cc
0.777 lb/in³
Wieland 1757 Wilaform Platinum
Platinum alloy without nickel, low-priced for all kinds of decoration productionApplications: chains, laminar decoration, pipes, tubingDental
Density 21.5 g/cc
0.777 lb/in³
CMW® ELKONIUM 301 platinum based alloy
Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (..